ITEM |
PROPERTY
|
REQUIREMENT
|
TEST METHOD |
1 |
Foam Type |
Polyether polyurethane foam impregnated with rigid conductive latex |
N/A |
2 |
Density kgm-3 |
35-55 |
BS 4443 Pt 1 Method 2 |
3 |
Tensile Strength kPa |
70 Minimum |
BS 4443 Pt 1 Method 3A |
4 |
Elongation @ Break % |
N/A |
BS 4443 Pt 1 Method 3A |
5 |
Loss in Tensile StrengthAfter Heat Ageing (%) |
30% Max Loss |
BS 4443 Pt 1 Method 3A 140oC for 16 hours |
6 |
Loss In Tensile StrengthAfter Humidity Ageing (%) |
30% Max Loss |
BS 4443 Pt 1 Method 3A105oC for 3 hours |
7 |
Compression Set (50% Compression) |
N/A |
BS 4443 Pt 1 Method 3A |
8 |
Volume Resistivity (ohms/m) |
250 Maximum |
BS 2044 Method 3 (100 Volts) |
9 |
Surface Resistance (K ohms) |
<10
|
Megger BM201 (100 Volts) |